| Material to be processed | Carbon steel/alloy steel/cast iron
< 20-30HRC |
Pre-hardened steel/quenched and tempered steel
< 35-48HRC |
Stainless steel/tool steel
< 25-35HRC |
|||
| diameter | Rotating speed | Feed rate | Rotating speed | Feed rate | Rotating speed | Feed rate |
| 3 | 10600 | 565 | 8500 | 370 | 7430 | 325 |
| 4 | 8000 | 575 | 6500 | 380 | 5570 | 335 |
| 6 | 5300 | 620 | 4200 | 405 | 3710 | 350 |
| 8 | 4000 | 615 | 3200 | 415 | 2785 | 365 |
| 10 | 3200 | 605 | 2500 | 390 | 2230 | 340 |
| 12 | 2650 | 605 | 2100 | 390 | 1855 | 340 |
| 16 | 2000 | 565 | 1800 | 370 | 1590 | 325 |
| 20 | 1600 | 555 | 1250 | 365 | 1115 | 315 |